Layer Thickness

Layer thickness is the height of each slice of material a printer adds, the step between one layer and the next along Z.

Every Layer Thickness article of the 3D Printing Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Layer thickness is the height of each slice of material a printer adds, the step between one layer and the next along Z. It sets the number of layers in a build, the step visible on a sloped face and part of the build time. Makers publish it per machine and parameter set. It is not a dimensional accuracy, a point the Formlabs tolerance guide makes plainly.

Typical Values

Published layer thicknesses run from 20 µm to about 150 µm across the machines in these resources. EOS runs 316L at 20, 40 and 80 µm (0.0008, 0.0016 and 0.0031 in) on the EOS M 290. The Formlabs Fuse series builds nylon in 110 µm (0.0043 in) layers, and EOS runs PA 2200 Balance at 120 µm (0.0047 in). The 3D Systems SLA 750 lists a layer resolution of 50 to 150 µm (0.002 to 0.006 in). Formlabs prints its Tough 2000 Resin V2 test parts at 100 µm (0.004 in).
Read More

Layer Count

Build height divided by layer thickness gives the number of layers. A Fuse build 300 mm (11.8 in) tall at 110 µm is about 2,730 layers. One 565 mm (22.2 in) tall is about 5,140 layers. If a 43-hour Fuse X1 build filled the chamber to the top, it would average about 30 seconds per layer. Formlabs does not state that build’s height, so the figure only shows the scale.

Detail and Speed

A thicker layer builds faster and gives up fine detail. On the EOS M 290, the 316L volume rate is 2.0 mm³/s at 20 µm and 3.7 mm³/s at 40 µm. It reaches 8.4 mm³/s at 80 µm. In US units that is 0.44, 0.81 and 1.85 in³ per hour. EOS calls the 80 µm rate more than double the 40 µm rate. Its 40/80 µm skin option assigns layer thickness by region of the part to cut total build time at the same surface quality.

Build Time

The volume rate turns layer thickness into hours by plain division. At 3.7 mm³/s, a 100 cm³ (6.1 in³) part needs about 7.5 hours of exposure, and at 8.4 mm³/s about 3.3 hours. That arithmetic leaves out recoating time, and EOS notes that the rate depends on part dimensions and skin thickness. For resin, the sources give no time per layer. The Somos EvoLVe 128 sheet gives only the cure exposure for a layer 0.254 mm (0.010 in) thick. Minimum wall thickness does not follow layer thickness in a simple way. On the EOS M 290, the 40 µm 316L set lists a 0.1 mm (0.004 in) minimum wall. The 20 µm set lists 0.3 to 0.4 mm (0.012 to 0.016 in). The sheet gives no reason, so a buyer asks which set a given wall was designed for before relying on either figure.

Surface Step

Layer thickness sets the stair step on a sloped or curved face. EOS notes a stair-step effect on sloping and curved 316L surfaces, and its later sheets chart roughness against build angle. The SLA 750 sheet lists layer resolution and dimensional tolerance on separate lines, because they describe different things. Reading 50 µm layers as a tolerance of ±50 µm (±0.002 in) reads the wrong line. In the Formlabs nylon study, XY stayed within ±0.2 mm (±0.008 in) of the average. That band is far wider than one 110 µm layer.

Powder Size

The coarsest powder in a metal bed is about as thick as a layer. EOS gives its 316L powder as 20 to 65 µm (0.0008 to 0.0026 in) and calls for a 63 µm (0.0025 in) sieve. The coarsest particles are about as thick as a 40 to 80 µm layer and 3 times a 20 µm layer. The sheet does not say how the distribution is matched to each layer thickness, so the matching is a question for the supplier. An order names the layer thickness with the parameter set, because the datasheet figures belong to that set.

3D Printing Defects in a Production Batch Traced to Their Cause

A defect in a printed batch is traced by its pattern, every part, one zone, one build or a slow trend across builds, and each pattern points to its own cause and evidence.

Reading a Defect by Its Pattern Across the BatchThe 2022 review sorts the sources of metal powder bed defects into three groups: defects transferred from the feedstock powder, defects formed in the interaction of the beam with powder and metal during melting, and defects created in post-processing such as heat treatment. It adds a fourth set of contributors around them: the equipment, powder handling and dispensing, and build preparation, meaning orientation and supports.

Orienting and Supporting a Part for SLA Printing

SLA orientation is set for the critical and cosmetic faces first, then checked for overhangs, cross section, trapped resin and support marks before anything is printed.

The Orientation Step in OrderThe order below follows Carbon's published assessment criteria for orientation and supports, with Stratasys's design guide filling in thresholds.

Surface Roughness of 3D Printed Parts by Process and Orientation

Process sets the floor of roughness and orientation moves it face by face, so a printed part's roughness note names the parameter, the face, its build direction and the finish.

Typical Ra and Sa of SLA, SLS, MJF and Metal SurfacesA review of as-printed polymer roughness in the International Journal of Advanced Manufacturing Technology collects dozens of studies by process. Another study printed one test artifact on four processes and measured them all the same way.

AlSi10Mg Aluminum Properties in Laser Powder Bed Fusion

Printed AlSi10Mg is stronger than the cast alloy as built, and the heat treatment named on the order decides how much strength is traded for ductility or conductivity.

AlSi10Mg Tensile and Yield Strength by Heat TreatmentThe first answer a buyer needs is the strength in each state the material is delivered in. Two makers publish it for their own systems and parameters, and their numbers are close enough to read together and different enough to show why the state and the source both travel with a figure.

How Many Parts Fit in One SLS or MJF Build

Chamber volume times packing density divided by part volume sets the count, and every term has a published limit.

How Many Parts Fit in a Powder Bed Fusion BuildPowder bed fusion, one of the seven process categories in ISO/ASTM 52900, builds parts inside a bed of powder that supports them, so a chamber can be filled in three dimensions and the parts need no support structures. The count that results is set by three quantities: the usable volume, the share of that volume that holds parts, and the volume of the part itself.

How Long a Batch of 3D Printed Parts Takes From Print to Pack-Out

A printed batch runs on four clocks, build, cooldown, finishing and inspection, and a stated lead time should show each.

Lead Time for a 3D Printed Batch Stage by StageThe calendar of a batch has the same skeleton in every process. Files are prepared and nested, the machine builds, the work cools or cures, parts are separated from what held them, and finishing and inspection follow.

Metal 3D Printing Stress Relief and Build Plate Removal Step by Step

Stress relieve metal parts on the plate, then cut, remove supports, anneal if needed and measure after the heat.

Metal Powder Bed Fusion Post-Build Steps in OrderThe post-build sequence for a part built on a plate has a stable shape across machine makers, because the stresses behave the same way. The sources agree on the order; they differ in how much of the detail they publish.

SLA Dimensional Tolerance by Feature Size

SLA tolerance is published as a percentage of feature size with a small floor, so a drawing writes bands and a post-cure condition and not one general figure.

SLA Tolerance Values Published by Two MakersTable 1 states the two specifications as their makers print them. Neither is a guarantee for a delivered part, and the Formlabs guide notes that the best way to judge a printer is to inspect real parts.

Tough SLA Resins as Stand-Ins for ABS and Polypropylene

Tough SLA resins match ABS on stiffness and strength but not on fracture energy or heat, so a part needs the row that governs its duty.

What a Tough SLA Resin Is Meant to ReplaceA tough SLA resin is a photopolymer that cures under ultraviolet light into a solid that bends before it breaks. Its makers aim it at the parts where earlier SLA resins cracked: snap fits, hinges, housings that are dropped and jigs that get clamped.

316L Stainless Steel Properties in Laser Powder Bed Fusion

Printed stainless steel is stronger along the layers and more ductile across them, and its size and finish depend on the parameter set and the heat treatment you name.

What 316L Is in a Laser Powder Bed Machine316L is a molybdenum-alloyed austenitic stainless steel. EOS markets its powder as a marine-grade steel with enhanced corrosion resistance in chloride environments, and it lists high ductility, high strength and high corrosion resistance as the main characteristics.

Send the 3D File of Your Printed Part

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with 3D Printing chosen.