Accura is the family of stereolithography resins made by 3D Systems for its SLA printers, ranging from general-purpose and clear grades to tough, flame-retardant and high-temperature ones.

Every Accura article of the 3D Printing Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Accura is the family of stereolithography resins made by 3D Systems for its SLA printers, ranging from general-purpose and clear grades to tough, flame-retardant and high-temperature ones. Accura grades appear in published studies and in makers’ application lists as the reference resins of industrial SLA.

Grades

3D Systems positions Accura 25 as polypropylene-like and general purpose, for snap-fit assemblies, styling parts, master patterns for urethane casting and parts normally machined from polypropylene or ABS, and notes that it was previously sold as VisiJet SL Flex for the ProJet 7000. Accura Xtreme and Accura Xtreme White 200 are described as tough resins that replace machined polypropylene and ABS. The SLA 750 page lists further grades, including a tough black resin rated UL 94 V0 and rigid composites.
Read More

Measured Properties

Accura ClearVue, also sold as VisiJet SL Clear, was tested on a ProJet 6000 HD by an Arizona State University study: 51.9 MPa (7,530 psi) tensile strength, 2,481 MPa modulus and 4.8 % elongation, against supplier values of 52 MPa, 2,550 MPa and 6 %. Build orientation had no significant effect on those properties, and strength rose markedly with age after printing.

Surface by Angle

The same ClearVue parts measured an Ra of 1.733 µm (68 µin) on the flat face, 2.686 µm (106 µin) at 30°, 2.546 µm at 60° and 1.649 µm (65 µin) on the vertical face, among the smoothest as-printed values in a review of polymer roughness.

Reading the Sheets

The Accura sheets mark their values as post-cured and publish ranges rather than single figures, so a figure taken from them carries its cure condition with it. A run in an Accura grade is specified by grade, printer and post-cure, and tested at a fixed age.

Orienting and Supporting a Part for SLA Printing

SLA orientation is set for the critical and cosmetic faces first, then checked for overhangs, cross section, trapped resin and support marks before anything is printed.

The Orientation Step in OrderThe order below follows Carbon's published assessment criteria for orientation and supports, with Stratasys's design guide filling in thresholds.

Surface Roughness of 3D Printed Parts by Process and Orientation

Process sets the floor of roughness and orientation moves it face by face, so a printed part's roughness note names the parameter, the face, its build direction and the finish.

Typical Ra and Sa of SLA, SLS, MJF and Metal SurfacesA review of as-printed polymer roughness in the International Journal of Advanced Manufacturing Technology collects dozens of studies by process. Another study printed one test artifact on four processes and measured them all the same way.

SLA Wash and Post-Cure Step by Step From Green Part to Finished Resin Part

Wash each resin for its own time, dry it fully, cure to the datasheet condition, then remove supports and measure.

SLA Wash, Dry, Cure and Support Removal in OrderThe part leaves the printer in a green state: polymerized enough to keep its shape, but with its reaction unfinished and a film of liquid resin over it. The order in which the finishing steps run is set by what each one needs from the one before.

ISO/ASTM 52927 Main Characteristics and Test Methods for AM Parts

The test methods standard links the characteristics of additive feedstock and parts to test procedures, and a buyer fixes the method, specimen, orientation and statistical basis in the order.

What ISO/ASTM 52927 Covers and Who It Is ForThe scope states that the document specifies the principal requirements applied to the testing of parts produced by additive manufacturing processes. It does three things.

Tough SLA Resins as Stand-Ins for ABS and Polypropylene

Tough SLA resins match ABS on stiffness and strength but not on fracture energy or heat, so a part needs the row that governs its duty.

What a Tough SLA Resin Is Meant to ReplaceA tough SLA resin is a photopolymer that cures under ultraviolet light into a solid that bends before it breaks. Its makers aim it at the parts where earlier SLA resins cracked: snap fits, hinges, housings that are dropped and jigs that get clamped.

Send the 3D File of Your Printed Part

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with 3D Printing chosen.

Request a Quote