Meaning
Inspection is the check of delivered parts against the limits an order sets, by a stated method and sample. ISO/ASTM 52901 names it as clause 4.4.4 of an order, under which the buyer agrees the method, the sampling and the specimens. ISO/ASTM 52900 holds the words for it under parts evaluation, clause 3.12. The vocabulary defines the terms, and the order defines the plan.Methods
Five methods cover most of a printed run. Gauge pins and go/no-go gauges answer whether every bore passes, and the sources publish no limit for them. An optical 3D scan compares overall form with the model and is the fastest method, though less precise than a coordinate measuring machine (CMM). A tactile CMM gives datum and feature dimensions, more slowly and more precisely. A stylus gives surface texture values. Computed tomography (CT) finds internal pores, voids and trapped powder, and it is the only method that sees inside the part.Read More
Stage of Measurement
The order of measurement matters on a printed part. A resin part is measured after post-cure, because the cure shrinks it. A nylon part is measured after unpacking at the agreed temperature, since Formlabs found that unpacking temperature changes warp. A metal part is measured after heat treatment. The EOS process data sheet for 316L-4404 at 40 µm gives a typical change of +0.02 % from that step. An order that names the inspection without its stage leaves the supplier free to measure before or after any of these steps.Full Inspection Features
A run of several hundred printed parts is rarely measured in full, and four kinds of feature earn every-part inspection. The first are features that mate with another part. The second are features sensitive to warp, such as long flat faces and thin walls. Datum features earn it because other measurements depend on them. So do dimensions that move after a step, such as those that shrink in post-cure. The sources give no standard sample size for a printed run, so the sampling plan is negotiated in the order.Statistics Behind a Limit
A datasheet value describes a population measured under a named recipe, and its sample count is part of the value. EOS reports its 316L defect percentage of 0.018 % from 45 samples. It reports its tensile data from 363 vertical and 246 horizontal specimens. A figure from 45 samples and one from 363 carry different weight. A statistic from one system does not carry to another, which is EOS’s own caution about its tolerance intervals.Surface Readings
Roughness is measured with a stylus, and the value depends on the measure and the method. EOS gives Ra and Rz for 316L on vertical faces and notes that the values depend on the measurement method. Its later sheets chart Sa against build angle without printing the numbers, so a buyer asks for the figure on the actual surface. Roughness also sits inside a dimension. An Ra of 13 µm (512 µin) is a third of a 0.04 mm (0.0016 in) tolerance band. The size read then depends on whether the gauge rides on the peaks or in the valleys.Inspection Plan
A plan names the features measured on every part, those measured on a sample, the sample size and the action when a part fails. It names the method for each critical dimension and the stage at which it is made. The first production part is inspected on every drawing feature before the rest of the run is built. A nylon order can add a check that every through-hole passes a named gauge pin. Weighing a few parts against the average is a practical check for trapped powder, though the sources give no pass threshold for it. Some characteristics cannot be tested without destroying the part. For those, feedstock records and process monitoring records stand beside the part tests, so lots can still be compared. ISO/ASTM 52927 splits testing into the feedstock, the process and the part for that reason.