Shot Peening

Shot peening is a finishing step for printed metal surfaces that EOS lists for 316L, lowering the as-built roughness.

Every Shot Peening article of the 3D Printing Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Shot peening is a finishing step for printed metal surfaces that EOS lists for 316L, lowering the as-built roughness. EOS gives vertical 316L faces as Ra 13 ± 5 µm (512 ± 197 µin) as built. After shot peening they measure Ra 5 ± 2 µm (197 ± 79 µin). EOS allows peening, like machining and polishing, either as built or after stress relief.

Surface Values

The May 2014 EOS sheet also gives Rz 80 ± 20 µm (3,150 ± 787 µin) as built. Polishing brings Rz below 1 µm (39 µin). Sloping and curved faces show a stair-step effect, and the values depend on the measurement method. A face that needs Rz below 1 µm needs polishing, not peening alone.
Read More

Effect on Dimension

Roughness sits inside a printed size. An Ra of 13 µm is a third of a 0.04 mm (0.0016 in) tolerance band. A gauge reads differently on the peaks and in the valleys. A thin-wall study measured vertical wall roughness of Ra 13.94 to 21.35 µm (549 to 841 µin) as laser power rose. Peening lowers the texture that a gauge has to ride over.

Clause Placement

ISO/ASTM 52901 places surface texture under clause 4.3.4 and post-processing under clause 4.4.5. A finishing step changes the surface that the earlier clause fixed. An order that names the inspection without its stage leaves the supplier free to measure before or after peening.

Surface Callout

The drawing marks each face as built, shot-peened, machined or polished. It gives the roughness value with its measure, Ra, Rz or Sa. The inspection of those faces follows the finishing step.

316L Thin Wall and Gap Dimensional Error in Laser Powder Bed Fusion

Printed metal walls and gaps land off the drawing by an amount the laser settings control, so a requirement names the parameter set, the gap needed and the finished size.

Thin Wall and Gap Error in 316L Laser Powder Bed FusionThe machine maker states accuracy as a band. EOS's sheet for 316L, dated May 2014, gives a typical achievable part accuracy of about ±20 to 50 µm (±0.0008 to 0.002 in) for small parts and about 0.2 % for large parts, and a minimum wall thickness of about 0.3 to 0.4 mm (0.012 to 0.016 in).

ISO/ASTM 52901 Requirements for Purchased Additive Manufactured Parts

The purchased parts standard lists what an additive parts order carries, from tolerances and feedstock to three acceptance stages, and leaves every value to the buyer.

What ISO/ASTM 52901 Asks a Buyer and a Supplier to ExchangeThe scope has three sentences and each one shapes how the standard is used. The first says the document defines and specifies requirements for purchased parts made by additive manufacturing.

316L Stainless Steel Properties in Laser Powder Bed Fusion

Printed stainless steel is stronger along the layers and more ductile across them, and its size and finish depend on the parameter set and the heat treatment you name.

What 316L Is in a Laser Powder Bed Machine316L is a molybdenum-alloyed austenitic stainless steel. EOS markets its powder as a marine-grade steel with enhanced corrosion resistance in chloride environments, and it lists high ductility, high strength and high corrosion resistance as the main characteristics.

Send the 3D File of Your Printed Part

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with 3D Printing chosen.

Request a Quote