Meaning
An acceptable imperfection is a departure from the ideal part that an order states a part may show and still pass. ISO/ASTM 52901 names acceptable imperfections and non-conformance as clause 4.3.8 of an order. The clause text is not public, so the order itself writes what counts as acceptable. A line left empty leaves the judgment to the supplier at inspection.Reference Figures
Datasheets give figures a buyer can write into the line. EOS reports an average defect percentage of 0.018 % from 45 samples on its 20 µm 316L set. It reports 0.1 % on the Core 40 µm set. As built, a 316L vertical face measures Ra 13 ± 5 µm (512 ± 197 µin), and sloped faces show a stair-step effect.Read More
Marks of the Process
Some marks belong to the process and are planned, not rejected. Supports leave rough contacts on metal that are ground by hand and marks on resin that are sanded. A drawing that names the faces allowed to carry them turns a dispute into a line of the order.Non-Conformance
Other faults fall outside any acceptable line. A metal part cut free of its plate before stress relief may fall out of flat beyond the drawing. A stainless part quenched more slowly than the datasheet asks can lose corrosion resistance to chromium carbides. In a 316L study, a gap drawn 0.20 mm (0.008 in) wide closed completely at high laser power, which the authors call a functional failure.Feature-by-Feature Line
An order writes, feature by feature, which flaws or marks are allowed and how each is measured. It pairs internal flaws with a method that sees them, computed tomography. The run’s acceptance record then lists the parts rejected and why, a list a mold maker uses when a tool takes over.